Investigation of Sulfur Crosslinking Interfacial of Natural Rubber (NR) Blending with Carboxyalted Styrene Butadiene Rubber (XSBR) Using X-Ray Absorption Spectroscopy

Chanaphan Lamlong, Wirach Taweepreda, Rattapong Nu-Mard, Prayoon Songsiriritthigul

Advanced materials research · 2015

The sulfur crosslinking films from Natural Rubber (NR), Carboxylated Stryrene Butadiene Rubber (XSBR) latices, and their blends have been investigated using X-ray absorption near-edge structure spectroscopy (XANES). The film was prepared by casting the latex compound on glass surface and heating at 120oC in a hot air oven for 10 minutes. The sulfur crosslinking density were studied by the XANES. This was done to provide the local geometry and electronic environment of sulfur bonding in the rubber networks. We found that the reversion takes place before the onset of oxidative processes at the sulfur bridges. Parallel to the oxidative processes, the production of cyclic sulfanes takes places. This relationship depends on the rubber compositions.

Influence of N-Doped TiO2 Nanocomposite Film on Hydrophilic Property of Rubber Dipping Former Surface

Mahamasuhaimi Masae, Lek Sikong, Kalayanee Kooptarnond, Wirach Taweepreda, Fumio Saito, Pichaya Pitsuwan

Key engineering materials · 2014

The objective of this study is to explore a method to improve hydrophilicity of the surface of formers that could be more easily dipped to produce high quality dipped rubber products. Photocatalytic TiO2 composite films were prepared by sol-gel method. Glass formers were coated with nitrogen doped TiO2 nanocomposite film by dipping method and annealed at 600°C for 1 h. Phase formation of TiO2 was characterized by XRD. Morphology of the TiO2 films was observed by using atomic force microscopy (AFM). Optical absorption of the films and degradation concentration of methylene blue had been measured employing UV-Vis spectrophotometer. The hydrophilicity of the thin films was determined in terms of the contact angles of water and NR rubber latex droplets on the coated TiO2 composite films under visible light irradiation. It was found from the experimental study that the TiO2 nano-composite film can improve wet-ability of the coated former surfaces.

Rheological Behavior Characterization of Natural Rubber Containing Different Gel

Saengchao Thongseenuch, Wirach Taweepreda, Krisda Suchiva

Advanced materials research · 2014

This research, natural rubber containing different gel contents were prepared by deproteinization and saponification treatment from high ammonium natural rubber latex. Deproteinization natural rubber was further treated as acetone extraction and then transesterification. It was founded that gel content and molecular weights of treated natural rubber were decreased and almost absented for transesterification treatment. Rheological respond on small amplitude oscillating shear (SAOS) and large amplitude oscillating shear (LAOS) deformation of treated natural rubber were captured by using rubber process analyzer (RPA 2000). Firs harmonic rheological properties, storage modulus, G and loss modulus, G decreased as gel content and molecular weight decreased. It was believed that gels, explicitly branching points, were destroyed after the natural rubber was deproteinized, transesterification, or saponification according to the molecular structure of natural rubber presumed by Tanaka et al, which functional groups contain protein and fatty acid are participated in branching to forming gel structure. It was concluded that gel content as the same as molecular structure of natural rubber could be characterized as rheological behavior.

Preparation of Positively Charged Membrane from Natural Rubber Latex Blending with Chitosan

Wirach Taweepreda, Supawadee Tuaybut, Sineenart Puangmanee, Tran Dang Khoa

Communications in Physics · 2014

Film formation of natural rubber latex (NRL) blended with various concentrations of chitosan was investigated. Atomic force microscopy (AFM) images clearly showed that the NRL film covered chitosan phase. Roughness of the films which was calculated from AFM image increases with increasing chitosan concentration. Miscibility of NRL and chitosan in solution was investigated by using dynamic mechanical thermal analysis (DMTA) and found that chitosan incorporated with NRL less than 40 weight percentage (wt%) was partially miscible. Films of the chitosan blending with higher NRL contents exhibited two peaks of glass transition temperatures. Interfacial polarization and dielectric properties of polymer films were improved with increasing NRL contents. Chemical structure of the blends was characterized by using attenuated total reflectance Fourier transform infrared spectroscopy (ATR-FTIR).

Electrospun Conditions of Poly(vinyl chloride) Nanofibrous Membrane Plasticized with Polyurethane

Kritsada Phatcharasit, Wirach Taweepreda, Kanoktip Boonkerd, Jin‐Kuk Kim

Jurnal Teknologi · 2014

Electrospun poly(vinyl chloride) (PVC) nanofibrous were prepared by electrospinning. Various concentration of polyurethane (PU) were added to PVC solution for plasticization of the electrospun nanofibrous. The pristine and plasticized nanofibrous were characterized by field emission scanning electron microscopy (FE-SEM), differencial thermal analysis (DTA), and thermogravimetry analysis (TGA), respectively. Thermal properties form DTA and TGA results indicated that the addition of PU decreased glass transition temperature (Tg) of PVC and increased heat resistance of PVC nanofiber. The dielectric constant of plasticized nanofibrous measured using precision LCR meter indicated that the membrane were dense.

Effects of precipitation temperature on the photochromic properties of h-MoO3

Phuriwat Jittiarporn, Lek Sikong, Kalayanee Kooptarnond, Wirach Taweepreda

Ceramics International · 2014

Feasibility Studies of Magnesium (II) Removal from Fresh Field Natural Rubber Latex Using Macroporous Cationic Exchange Resin

Sineenart Puangmanee, Wirach Taweepreda

Advanced materials research · 2013

The presence of magnesium ions (Mg2+) in fresh field natural rubber latex (FF-NRL) is a major concern for concentrated production. In general, Mg2+ is reduced by adding diammonia hydrogen orthophosphate (DAP) to FF-NRL. The reaction rate between DAP and Mg2+ in NRL is very slow and is the cause of waste latex sludge, waste time for more than 12 hours, and chemicals loss. Moreover, the waste latex sludge is toxic and has to be treated. In this research, the possibility of using cationic exchange resin to remove Mg2+ from the FF-NRL was investigated. The experiment was carried out by comparison the efficiency of difference commercial exchange resin on Mg2+ reduction rate after immersing in FF-NRL. The results were found that macroporous cationic exchange resin adsorped Mg2+ with highest rate. The Mg2+ content of NRL reduced to 100 ppm after immersing macroporous cationic exchange resin in FF-NRL for 6 hours. The performance of cationic exchange resin was increased after regenerate process with acid and can be used for further to reduce Mg2+ in FF-NRL. The morphology of cationic exchange resin was investigated using scanning electron microscope (SEM).

Green Lightweight Concrete Made from Natural Para Rubber Product

Duangden Raksritong, Danupon Tonnayopas, Wirach Taweepreda, Manoon Masniyom

Key engineering materials · 2013

Para Rubber Seed Shell (PRSS) as a coarse aggregate and coated by vulcanization and mixing epoxy natural rubber (ENR) was investigated. Natural rubber latex (60% DRC) was applied in two stages. Firstly stage, synthetic natural latex (ENR-35) solution was coated on the first layer of PRSS. After that, PRSS was coated by vulcanization in second layer. Then, pre-wetting was performed before mixing or casting the concrete for 5 days. Finally, CPRSS (Coated Para Rubber Seed Shell) was produced. The CPRSS aggregate was cast as self consolidation concrete (SCC) with different ratios of ordinary Portland cement: sand: CPRSS for 0.8-1: 0.6-0.85: 0.04-0.12 by weight, respectively and constant water/binder ratio at 0.45 throughtout this study. The ENR-35 was also used about 5% of the water content. However, the concrete was wrapped with polyvinyl sheet to prevent moisture loss during setting and curing in ambient temperature (29°C, 84%RH) for 28 days. The fresh concrete to slump test, harden concrete with bulk density and compressive strength of whole formulations was carried out to determine. The test result A8 indicted that the most ingredient suitable mixture of SCC involed cement: sand: CPRSS of 1:0.94:0.046. The SCC contained the slump as 120 mm, bulk density about 1916 kg/m3 and compressive strength was 37 MPa. Its was met specification of structural lightweight concrete. This beneficiation of SCC is also product as the green innovation building in terms of construction materials and resources, leaving minimal environmental impact, and having energy saving and eco-friendly materials.

Electrospun Epoxidized Natural Rubber with Poly(vinyl chloride) (ENR-PVC) Nanofibrous for PEMFC Applications

Kritsada Phatcharasit, Wirach Taweepreda, Kanoktip Boonkerd, Jin Kuk Kim

Advanced materials research · 2013

Various electrospun epoxized natural rubber / poly (vinyl chloride) (ENR/PVC) blend nonwoven membranes were prepared by electrospinning technique. Various concentration of epoxidized natural rubber (ENR) solution in N,N-dimethylformamide (DMF) were directly added to PVC solution for plasticization of the electrospun nanofibrous. Differencial thermal analysis (DTA), thermogravimetry analysis (TGA), fourier transfrom infrared spectroscopy (FT-IR), and scanning electron microscopy (SEM) were used to characterize the pristine and plasticized nanofibrous. DTA results indicated that the addition of ENR resulted in the shifting of glass transition temperature (Tg) towards lower temperatures. The blending of PVC with ENR is thermodynamically incompatible.

Fabrication and Characterization of Epoxidized Natural Rubber-Chitosan Membrane

Wirach Taweepreda, Anuchit Wichianchom

Advanced materials research · 2013

The membranes obtained from the mixtures of epoxidized natural rubber latex (ENR) and chitosan solution were prepared and characterized. The chemical structure of the membrane was confirmed by ATR-FT-IR spectroscopy and found the peak at 1315 and 1155 cm-1 indicated ether linkage was formed between epoxide group and chitosan corresponding with an enhancement of their mechanical properties which were observed using dynamic mechanical thermal analysis (DMTA). The dielectric properties and ionic conductivity of membrane were investigated using LCR meter and found that the ionic conductivity was increased with increasing the chitosan content.

Novel Process in Preparation of Deproteinized Natural Rubber Latex

Prapaporn Boonme, Wirach Taweepreda, Wiwat Pichayakorn

Advanced materials research · 2013

Natural rubber latex (NRL) tapped from Hevea brasiliensis is composed of cis-1,4-polyisoprene as the major polymer which provides several desirable physical properties which make it to be interesting in pharmaceutical formulations. However, the International Union of Immunological Societies (IUIS) has reported about latex allergies caused by 14 NRL proteins (Hev b1-14). This problem can be coped with deproteinization of NRL in order to obtain deproteinized natural rubber latex (DNRL). This study aimed to prepare DNRL by novel process which was easy to perform and used pharmaceutical acceptable agents. The obtained DNRL was assayed for remained protein amount in form of nitrogen content by Kjeldahl method. Its physical properties were characterized. Its stability was also physically investigated. The DNRL was tested for the skin irritation in 3 rabbits. It was found that the protein amount of DNRL was 0.257% while the initial protein amount of fresh NRL was 1.531%. Hence, the protein was removed for 83.21%. DNRL had the average pH of 7.27. Both protein content and pH value implied that DNRL should be safe for skin application. DNRL possessed Newtonian flow with low viscosity which should be easy for mixing with other components in the further pharmaceutical formulations. The particle size, polydispersity index (PI), and zeta potential of DNRL were 441.0 nm, 0.240, and -42.53 mV, respectively, indicating narrow size distribution and physical stability. The dry rubber content and total solid content of DNRL were controlled as 39.55% and 40.72%, respectively. The suitable storage condition of DNRL was at 2-8°C in tight containers where DNRL could be kept for longer than 4 months. Very slightly irritation with no allergy caused by DNRL was observed in the tested rabbits. It could be concluded that this deproteinization process was easy and the prepared DNRL by this process was suitable and safe for using in further pharmaceutical and cosmetic formulations.

Cosmetic Pore Packs from Deproteinized Natural Rubber Latex

Wiwat Pichayakorn, Prapaporn Boonme, Wirach Taweepreda

Advanced materials research · 2013

Natural rubber latex (NRL) from Hevea brasiliensis consists of cis-1,4-polyisoprene that have many excellent physical properties such as high elasticity, tensile strength, and easily film-forming. However, some proteins in NRL can cause allergy. Hence, this research aimed to prepare cosmetic pore packs from deproteinized NRL (DNRL) that was prepared in-house by enzyme treatment and centrifugation processes. The properties of DNRL were evaluated in terms of amount of remained protein, pH, particle size, polydispersity index, and zeta potential. This DNRL was then formulated the pore pack products by mixing with the other ingredients and casting to the film form. An appropriate pore pack formulation composed of sodium alginate and polyvinylpyrrolidone K30 mixed with DNRL to produce films with good properties. Hydroxypropylmethylcellulose was also added to another formulation for improving toughness of the films. Both products had similar appearance and physical properties such as thickness, uniformity of weight, pH, tensile strength, and elongation at break, but lower peel strength comparing with the commercial pore pack product. These films showed good flexibility, softness, and toughness. After storage at room temperature for a month, there were no different in appearance and pH that presented good stability. The obtained pore packs also exhibited desirable characteristics with acceptable volunteer satisfactions. However, they should be improved for more adhesiveness in further study. In conclusion, DNRL could be used as major component for cosmetic pore pack preparations.

Separation and Characterization of Minerals from Centrifuged Waste Latex Sludge

Wirach Taweepreda

2013

Preparation and Properties of Electrospun PVC Nanofiber

Kritsada Phatcharasit, Wirach Taweepreda, Kanoktip Boonkerd, Jin Kuk Kim

Advanced materials research · 2013

Nanofibrous membranes based on poly (vinyl chloride) (PVC) were prepared by electrospinning. The morphology of nanofibrous was observed under field emission scanning electron microscope (FE-SEM) and effects of instrument parameters including electric voltage, tip to collector distance, and solution parameters such as PVC concentration and mixed solvent of THF and DMF (50:50) were evaluated. The beads on the fiber were formed with low concentration of PVC. The dielectric constant, thermal properties and crystallinity of the electrospun membranes were characterized by precision LCR meter, and differential thermal analysis (DTA), respectively. It was found that smooth surface of electrospun PVC nanofiber had a high ionic conductivity and their thermal properties were improved comparing with PVC sheet.

Preparation of Peel-off Mask from Deproteinized Natural Rubber Latex

Wiwat Pichayakorn, Prapaporn Boonme, Wirach Taweepreda

Advanced materials research · 2013

The aim of this research was to develop the peel-off mask in paste form which can be applied to the face and then formed removable thin film. Deproteinized natural rubber latex (DNRL) from Hevea brasiliensis was used as the major film former. After deproteinization by alcalase enzyme treatment, the protein amount was 0.257% that reduced from the initial amount of 1.531%. The appropriate types and amounts of additives were studied by optimization design. The product compatibility and stability were evaluated. The addition of active ingredients for skin nourishing was also investigated. The suitable formulation composed of DNRL, polyvinyl alcohol (PVA) and methylcellulose (MC) as film formers, propylene glycol (PG) and glycerin as plasticizer, Tween 80 as stabilizer, Paraben concentrate as preservative, and other active ingredients including tocopheral acetate, aloe vera, jojoba oil, and tamarind extract. The product was white viscous paste with the pH of 5.69, viscosity of 28,100 cps as pseudoplastic flow behavior, and stable when kept in well-close container at room temperature for more than 1 month. The product in situ film was good elasticity indicated by initial modulus (0.96 MPa), tensile strength (0.208 MPa) and elongation at break (105.6%). Skin irritation in rabbit skin was very slightly which showed the small rash skin but could recover soon. The complacency test in 50 healthy volunteers showed the good results with no irritation effect. In conclusions, DNRL could be prepared peel-off mask product with good properties.

Propranolol Hydrochloride Extended-Release Matrix Tablets Using Natural Rubber Latex as Binder

Kamon Panrat, Prapaporn Boonme, Wirach Taweepreda, Wiwat Pichayakorn

Advanced materials research · 2013

Matrix is one of the most interesting drug delivery systems to control drug release in pharmaceutical dosage forms. Natural rubber latex (NRL) from Hevea brasiliensis consists of cis-1,4-polyisoprene as the major polymer. It presents interesting physical properties such as easy to manipulate, low cost, high mechanical resistance, and insoluble in water. The aim of this study was to use the NRL as binder in matrix tablets for controlling the release rate of drug. NRL, sodium carboxymethylcellulose, olive oil, Tween 80, and lactose were used as polymer, adsorbent, plasticizer, surfactant, and diluent, respectively. Propranolol hydrochloride was used as a model drug. Propranolol hydrochloride matrix tablets were prepared by conventional heat-melting method. The in vitro release of drug from matrix tablets was determined by UV-Vis method according to dissolution test under Propranolol Hydrochloride Tablets USP30-NF25 monograph. Morphology of propranolol hydrochloride matrix tablet before and after released study was observed by scanning electron microscopy (SEM). It was found that NRL matrix tablets could control the drug release up to 12 hours. The release profiles were best fitted with Higuchi model. NRL amounts affected the properties of the propranolol hydrochloride matrix tablets. Increasing the NRL quantity in the matrices provided the decrease of release rate of drug. SEM photographs showed the number, size, and distribution of pore in propranolol hydrochloride matrix tablets that depended on amount of NRL addition. These results confirmed that NRL was possible to use as binder for matrix tablets in oral drug delivery systems.

Rubber recovery from centrifuged natural rubber latex residue using sulfuric acid

Wirach Taweepreda

DOAJ (DOAJ: Directory of Open Access Journals) · 2013

Waste latex sludge from centrifuged residue, which is a null by-product of concentrated latex manufacturing, wasdigested to retrieve the rubber by using sulfuric acid. It was found that the acid concentration and digestion time have aneffect on the amount and purity of the retrieved rubber. Sulfuric acid at concentrations of more than 10% by weight with adigestion time of 48 hours completely digested waste latex sludge and gave rubber 10% by weight. The quality of the retrievedrubber was examined for Mooney viscosity (MV), plasticity retention index, nitrogen content, and ash content. The averagemolecular weight of the retrieved rubber, using gel permeation chromatography, was lower than that of normal natural rubber(NR) which corresponds with the MV and initial plasticity (Po). The molecular structure from Fourier transform infraredspectroscopy (FT-IR) indicated that the retrieved rubber surface is wet composed with hydroxyl functional ended group.The residue solution was evaporated and crystallized. The structure of crystals was determined using power X-ray diffractometer.

Efficacy of a Rubber Seated Cushion for Pressure Ulcer Prevention: An experimental Study /Wipa Sae-sia, Wirach Taweepreda and Luppana Kitrungrote

Wipa Sae‐Sia, Wirach Taweepreda, Luppana Kitrungrote

2013

Improved Deproteinization Process for Protein-Free Natural Rubber Latex

Wiwat Pichayakorn, Jirapornchai Suksaeree, Wirach Taweepreda

Advanced materials research · 2013

Hev b1-14 type proteins in natural rubber latex (NRL) have been identified as allergens in immunogenic responses. Several methods have been developed to reduce these proteins from NRL such as enzyme treatment, centrifugation, creaming, simple or ultrasonic leaching, and chlorination. In this work, the improvement of deproteinization of NRL was developed using the combination of enzyme treatment and leaching processes. The fresh NRL was incubated with 0.2 phr proteolytic alcalase enzyme, and preserved with 2%v/v paraben concentrate in the presence of a 2%v/v sodium lauryl ether sulfate (SLES) as a surfactant at 37°C for 24 hours, and then centrifuged. The upper rubber mass was then leached for three times with either distilled water, a 1%v/v SLES solution, or a mixture of 1%v/v SLES and 2.5%v/v ethanol, and then finally re-dispersed in distilled water. It was found that the increasing process of leaching with either 1%v/v SLES or a mixture of 1%v/v SLES and 2.5%v/v ethanol had the higher efficacy to reduce the remained protein in deproteinized NRL (DNRL). The best deproteinized process was the enzyme treatment and followed by the three times leaching process with a mixture of 1%v/v SLES and 2.5%v/v ethanol, that could completely reduce the proteins in DNRL to 0%. This DNRL had the pH value, viscosity, dry rubber content, and total solid content of 7.41, 13.82 cps, 42.57%, and 44.63%, respectively. Its particle size was 626.23 nm with low polydispersity index of 0.16. The negative charge of SLES could increase the higher negative charge of DNRL to-63.20 mV that exhibited very good physical stability during storage. In conclusions, the combination of enzyme treatment and leaching process with both SLES and ethanol was successful to produce the protein-free DNRL. This DNRL could be further used for several applications including medical skin products.

Polyethylene Thin Film Coating Preventing the Degradation of Natural Rubber

Wirach Taweepreda, Kritsada Phatcharasit

Engineering Journal · 2012

In this research, natural rubber (NR) was directly mixed with polyethylene (PE) and was compressed at 150 o C. The PE was then separated and migrated to form a thin film on the rubber surface during the vulcanization process. The tensile properties of composite film were rising with increasing the PE contents from 15 to 150 phr as well as the ozone aging properties. The surface topography of the composite film was examined by using scanning electron microscopy (SEM) and was found that the PE form lamellar crystallites on the rubber interface after ozone treatment. The effect of PE on NR crosslinking was also investigated using S K-edge XANES Spectroscopy.

Self-assembled nanometric spacer on surface of natural rubber composited with TiO2

Wirach Taweepreda, Kritsada Phatcharasit

World Journal of Engineering · 2012

The dispersion of titanium dioxide (TiO2) was mixed with natural rubber latex (NRL) and other additives before casting on glass slide. The dispersion of TiO2 (75% by wt.) were prepared using high pressure homogenizer by varying the concentration of stabilizer, poly (ethylene glycol) (PEG). The results were found that PEG can disperse TiO2 in water phase and the mechanical properties of NRL film composited with TiO2 dispersion is enhancement with increasing the PEG concentration. The effects of the stabilizer and NRL compounding on composited films properties were discussed using surface morphology. The morphology of TiO2 dispersion and composited NRL films were investigated using scanning electron microscopy (SEM) and atomic force microscopy (AFM).

Film Formation of Inclusion Complexes between Acetyl-Beta-Cyclodextrin and Chitosan

Wirach Taweepreda, Pikul Wanichapichart

Advanced materials research · 2012

In this research, the films which were prepared from inclusion complexes (ICs) of acetyl-beta-cyclodextrin (Acetyl-β-CD) with chitosan were characterized and the membrane properties were investigated. Acetyl-β-CD either improved the solubility of chitosan or increased the salt rejection of the membrane. The crystalline ICs, were formed and found on the membrane surface. There were isolated and characterized by scanning electron microscopy (SEM), X-ray diffraction and atomic force microscopy (AFM). The stability and conformation of the inclusion complexes in solvent and limited number of acetyl-β-CD threaded on chitosan molecules were studied and compared the results on a molecular level of the pseudopolyrotaxane.

Removal of organic impurities in waste glycerol from biodiesel production process through the acidification and coagulation processes

Qiao-guang Xie, Wirach Taweepreda, Charongpun Musikavong, Chaisri Suksaroj

Water Science & Technology · 2012

Treatment of waste glycerol, a by-product of the biodiesel production process, can reduce water pollution and bring significant economic benefits for biodiesel facilities. In the present study, hydrochloric acid (HCl) was used as acidification to convert soaps into salts and free fatty acids which were recovered after treatment. The pH value, dosages of polyaluminum chloride (PACl) and dosage of polyacrylamide (PAM) were considered to be the factors that can influence coagulation efficiency. The pH value of waste glycerol was adjusted to a pH range of 3-9. The PACl and PAM added were in the range of 1-6 g/L and 0.005-0.07 g/L. The results showed best coagulation efficiency occurs at pH 4 when dosage of PACl and PAM were 2 and 0.01 g/L. The removal of chemical oxygen demand (COD), biochemical oxygen demand (BOD(5)), total suspended solids (TSS) and soaps were 80, 68, 97 and 100%, respectively. The compositions of organic matters in the treated waste glycerol were glycerol (288 g/L), methanol (3.8 g/L), and other impurities (0.3 g/L).

Oxidative Degradation Monitoring of Natural Rubber Using S K-Edge X-Ray Absorption near-Edge Spectroscopy (XANES)

Wirach Taweepreda, Wanwisa Limphirat, Prayoon Songsiriritthigul

Advanced materials research · 2012

In this work, we present the results of sulfur crosslinking and degradation in natural rubber (NR) studied by X-ray absorption near-edge structure spectroscopy (XANES). Sulfur K-edge XANES spectra has been collected and analyzed to provide the geometry and electronic environment of sulfur crosslinks during vulcanization and degradation processes by ozone aging. We found that reversion took place before the onset of oxidative process at the sulfur bridge. Parallel to the oxidative process, the production of cyclic sulfanes took places. This physico-chemical properties which were calculated from S K-edge XANES spectra were correlated with the mechanical of NR films by varying accelerator type. The accelerator zinc diethyldithiocarbamate (ZDEC) gave highest film strength when compared with other accelerators: N-cyclohexylbenzothiazole sulfenamide (CBS), 2,2' dibenzothiazyl disulfide (MBTS), and tetramethylthiuram disulfide (TMTD).

Preparation of Deproteinized Natural Rubber Latex and Properties of Films Formed by Itself and Several Adhesive Polymer Blends

Wiwat Pichayakorn, Jirapornchai Suksaeree, Prapaporn Boonme, Wirach Taweepreda, Garnpimol C. Ritthidej

Industrial & Engineering Chemistry Research · 2012

This work aimed first to prepare deproteinized natural rubber latex (DNRL) and investigate the properties of films after it was blended with various adhesive polymers: hydroxypropylmethyl cellulose (HPMC), methyl cellulose (MC), sodium carboxymethyl cellulose (SCMC), poly(vinyl alcohol) (PVA), poloxamer 407, and sodium alginate. The second aim was to identify the films that would be the best for medical and pharmaceutical applications. Dibutyl phthalate (DBP), diethyl phthalate, dibutyl sebacate, triethyl citrate, and glycerin (GLY) were used as plasticizers to improve the elasticity and adhesiveness of the novel materials. DNRL was prepared by proteolytic alcalase enzyme treatment, followed by centrifugation. The DNRL was virtually free of protein, produced no significant reaction in the rabbit skin irritation test, and formed a good elastic film, but it had low skin adhesive properties. Blending DNRL with several polymers produced better films with different elastic and adhesive properties. Moisture uptake and swelling tests indicated that its films provided increasing hydrophilicity when blended with several polymers. SEM showed homogeneous films, and water hydraulic permeability tests indicated some porosity in matrix films. Blending DNRL with HPMC or PVA and DBP or GLY produced films with the best potential for novel materials. FT-IR, DSC, and XRD studies indicated the compatibility of the blended ingredients. In conclusion, DNRL blends could be used suitably for medical and pharmaceutical applications.

Page 3 of 4

Analytics cookies

This site uses Google Analytics to see aggregate usage — visitor counts and which pages get attention. It only runs if you accept.

No choice made yet